Tikkurila Temacoat GPL 2k Floor & Metal Epoxy Paint with Hardener is a two-component, amine-adduct-cured epoxy topcoat for concrete floors and steelwork. A finishing coat for surfaces taking heavy abrasion and chemical attack, it resists +150°C dry heat and chemically active gases and dust. Stocked as a 10L kit, tinted to any RAL or NCS colour.
What it's for
Steelwork, tanks and bridges: conveyors, paper machines and plant in the wood processing and chemical industries.
Concrete in process industries: CE marked to EN 1504-2.
Immersion: water, oil and dilute non-oxidising acid, alkali and salt solutions, up to +60°C.
Coverage and film thickness
50 microns dry film (90 microns wet): 11.0 m²/L theoretical.
100 microns dry film (185 microns wet): 5.5 m²/L theoretical.
So a 500 m² floor takes about 91 litres mixed at the 100 micron build, 45 at 50 microns. Theoretical figures, so order above them.
Mixing, pot life and drying
Mixing ratio: 3 parts base to 1 part hardener by volume. Stir each separately, then power-mix.
Pot life: 5 hours from mixing.
Airless spray: thinned about 0 to 10% with Thinner 1031, 0.011 to 0.017 inch tip, 120 to 160 bar.
All of Tikkurila's drying times are measured at 60 microns dry film:
Dust dry: 3 hours at +10°C, 2 at +23°C, 1 at +35°C.
Touch dry: 10 hours at +10°C, 5 at +23°C, 2 at +35°C.
Recoat: 10 hours at +10°C, 4 at +23°C, 2 at +35°C.
Recoat before immersion: 32 hours at +10°C, 16 at +23°C, 8 at +35°C.
Film thickness, humidity and ventilation all move those times, and the 100 micron build above is nearly double that basis, so allow longer.
Conditions it needs
+10°C minimum: air, surface and paint, right through application and drying. An unheated Irish slab is below it overnight from October on.
Relative humidity 80% maximum: through application and drying, with good air movement in confined areas.
Steel at least 3°C above dew point.
Concrete dry, at least 4 weeks old, internal humidity no higher than 97%: g